Condensate Polishing Resins and Ready to Use Mixed Bed Resins

Suqing
Ionic Form
Total Capacity min(meq/ml)
Water Retention (%)
Shipping Weight (g/ml)
Particle Size (mm)
Maximum Reversible Swelling
Remarks


Condensate Polishing Resins

D003NJ
Na
1.90
42~48
0.80~0.85
0.70~0.90
Na→H5~8%
Specially designed for condensate polishing. Excellent resistance to physical breakage, osmotic shock fracture and oxidation. The flow rate can be up to 120 m/h.
D203NJ
Cl
1.40
42~48
0.66~0.72
0.50~0.70
Cl→OH 15%


Ready to Use Mixed Bed Resins

MBS 1
99% H+
95% OH-
0.6
/
0.71~0.74
/
/
001X7H 40%, 201X7OH 60%
MBS 8
0.5
/
0.71~0.74
/
/
001X8H 40%, 201X4OH 60%
MBS 10
0.5
/
0.72~0.76
/
/
001X7H 50%, 201X7OH 50%
MBS 45
0.5
/
0.72~0.76
/
/
001X8H 50%, 201X4OH 50%
MBS 55
0.45
/
0.72~0.76
/
/
001X8H 45%, 201X7OH 55%
MBS 73
0.6
/
0.7~0.74
/
/
001X8H 33%, 201X7OH 66%
MBS 74
0.6
/
0.71~0.74
/
/
001X8H 40%, 201X7OH 60%
MBS 75
0.5
/
0.72~0.76
/
/
001X8H 50%, 201X7OH 50%

Copyright(C)2005,suqing Group All Rights Reserved. Supported by ChemNet ChinaChemNet Toocle